FREKOTE 700-NC

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

Frekote 700-NC GL

Main features

  • No Chlorinated Solvents
  • High Gloss Finish
  • No Contaminating Transfer

Product Description

LOCTITE® FREKOTE 700-NC™ is a solvent-based polymer mold release coating designed for composite and molded polymer manufacturing processes. This room-temperature-curing release agent delivers a clear, colorless coating that provides high gloss, high slip, and clean release characteristics without contaminating transfer or mold build-up. Suitable for mold temperatures from 13°C to 135°C, it is used with epoxy resins, polyester resins, thermoplastics, rubber compounds, and other molded polymers where consistent release performance is required. Its cured thermal stability of up to 400°C supports demanding molding environments and repetitive production cycles.

Key features

  • High-performance mold release: Provides reliable release for epoxies, polyester resins, thermoplastics, rubber compounds, and most molded polymers.
  • Clean, non-transfer coating: Delivers high gloss and high slip characteristics with no contaminating transfer or mold build-up.
  • Wide operating temperature range: Applicable at mold temperatures from 13°C to 135°C with cured thermal stability up to 400°C.

Applications / Suitable for

  • Composite molding operations
  • Epoxy resin processing
  • Polyester resin molding
  • Thermoplastic molding
  • Rubber molding applications
  • Mold release coating programs requiring high-gloss finishes
Product Family

215434

1 gal - Can | Clear
1. Select Package Type
2. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Unit of measure Can
Net weight 2.8 kg
Gross weight 3 kg
Dimensions 20.3 x 11.4 x 25.4 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear, colorless
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.755 to 0.764

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties and processing characteristics for LOCTITE® FREKOTE 700-NC™.

Property Value Unit Method / condition
Appearance Clear, colorless — As supplied
Chemical Type Solvent-based polymer — Product description
Specific Gravity 0.755 - 0.764 — @ 25°C
Application Temperature 13 - 135 °C Mold surface temperature
Cure Type Room temperature cure — Typical processing condition
Technical properties

After-processing / final-state properties

Published final-state performance characteristics available from supplied source data.

Property Value Unit Method / condition
Cured Thermal Stability ≤400 °C Published cured-state characteristic

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers