DOWSIL HC 1000 Gray Conformal Coating

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DOWSIL HC 1000 Silicone Adhesive

Main features

  • One-Part, Solventless Silicone Coating
  • Room-Temperature Adhesive Cure
  • 21 kV/mm Dielectric Strength

Product Description

DOWSIL™ HC 1000 Gray Conformal Coating is a one-part, solventless polydimethylsiloxane conformal coating developed for environmental and dielectric protection of printed circuit board assemblies. The high-viscosity material cures through exposure to atmospheric moisture at room temperature and reaches a typical tack-free state in 11 minutes at 25°C. After cure, it forms a soft, low-stress silicone elastomer that helps protect assemblies exposed to moisture, vibration and harsh operating environments. Its gray pigmentation can hinder component identification, while controlled volatility supports use around sensitive electronic devices. The coating also carries a UL 94 V-0 flammability classification.

Key features

  • Solventless, one-part formulation: Supplied as a ready-to-use silicone coating with 97.6% typical non-volatile content.
  • Soft, low-stress cured elastomer: Typical Shore A hardness of 24 supports stress-relieving protection of delicate components and interconnections.
  • Controlled volatility and flame classification: Designed for use around sensitive devices and classified UL 94 V-0.

Applications / Suitable for

  • Printed circuit board system assemblies
  • Appliances requiring dielectric insulation
  • Electronic assemblies requiring protection from moisture, vibration and harsh operating environments

Technical Specifications

General Properties
Color
The color
Gray
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
One
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.07
Physical Properties
Tack-Free Time
11 minutes
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
12,000 mPa.s
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
21 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
2.0 E15 Ohms⋅cm
Thermal Properties
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
94 V0

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of DOWSIL™ HC 1000 Gray Conformal Coating in its as-supplied condition. Values are not intended for preparing specifications.

Property Value Unit Method / condition
Components One — As supplied
Color Gray — Typical
Viscosity 12,000 cP (mPa·s) Typical
Non-volatile content 97.6 % Typical
Tack-free time 11 minutes Room-temperature cure at 25°C
Room-temperature cure time 0.5 hours Cure time depends on application method, film thickness, temperature and humidity
Technical properties

After-processing / final-state properties

Typical properties of the cured coating. Values are not intended for preparing specifications or for use alone as design values.

Property Value Unit Method / condition
Specific gravity 1.07 — Cured
Durometer hardness 24 Shore A Cured
Dielectric strength 525 (21) V/mil (kV/mm) JIS K 6249
Volume resistivity 2.0 × 1015 ohm·cm JIS K 6249
Dielectric constant 3.2 — At 1 MHz
Dissipation factor 0.003 — JIS K 6249; at 1 MHz
Flammability classification V-0 — UL 94