ABLESTIK 8361J
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Excellent dispensability
- 1mil Spacers
- Minimal voiding
Product Description
LOCTITE ABLESTIK 8361J die attach epoxy adhesive is designed for high reliability packaging applications. This electrically conductive epoxy offers high purity and minimal resin bleed, together with a low amount of condensable volatiles.
LOCTITE ABLESTIK 8361J exhibits minimal tailing and stringing, along with minimal voiding. It stands out for its excellent strength retention after temperature and humidity exposure and its moderate stress absorption properties. Please note that this product contains 1mil silver spacers for a more controlled bondline.
Cure Schedule
- 1 hour @ 175°C
- 30 minute ramp to 115°C + 30 minutes @ 175°C