ABLESTIK 2053S

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Loctite Ablestik 2053S

Main features

  • Low stress
  • Non Conductive
  • Use in Array packaging

Product Description

LOCTITE ABLESTIK 2053S is a polymer filled, hybrid non conductive die attach adhesive with low warpage, high adhesion, low stress and low moisture uptake, designed for use in array packaging. It exhibits great optical performance, complimented by high transmittance, high Optical density and HRI and good adhesion to various interfaces such as EMC, engineering plastic, glass and metals.  It is a low modulus, chip bonding, die attach paste for larger die size that works, among others, for chip bonding on FR4 substrates. It is considered a low modulus epoxy alternative to QMI536NB with less tendency to bleed than Bismaleimide containing, QMI materials. The modulus is ~3 times lower so this can be critical for wire bonding small die sizes.

LOCTITE ABLESTIK 2053S offers relatively high thermal conductivity with stable optical performance, good temporary bonding and minimal shift and tilt post reliability. It has been successfully used for the ASIC (Application Specific Integrated Circuit) attach of automotive optical sensors, as a receiver Die attach for 3d sensing modules.

 

Cure Schedule

  • 30 minute @ 175°C + 15 minutes @ 175°C
Product Family

213639

10 cc - Syringe | Red
1. Select Package Type

Loading pricing…

Packaging
Unit of measure Syringe
Net weight 10 g
Gross weight 19.02 g
Dimensions 9.1 x 2.3 x 3 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
24 hours
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
-21 °C
Weight Loss @ 300°C
2.3 %
Chemical Properties
Moisture absorption
1 %
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
2.5
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
13,000 mPa.s

Additional Information

As part of Henkel’s commitment to becoming 100% PFAS-free by 2027, 2053S will be phased out.

  1. Is 2053SNP a replacement or an alternative?
    Henkel has confirmed that 2053SNP should be considered the direct replacement for 2053S. It has been formulated to match the performance of the existing product, with the only change being the removal of the PFAS-containing anti-bleed agent. No significant property differences are expected (TDS comparison confirms this).
  2. Will this affect other Henkel PFAS-containing materials?
    Yes. This transition is part of a broader portfolio-wide PFAS removal initiative. Any products containing PFAS are being reviewed and will follow a similar process.
  3. Will a PCN / End-of-Life notice be issued?
    Yes. Henkel will issue the official EOL notification in January 2026, with a Last Time Buy window during December 2026.
    Given the 12-month shelf life, qualification of 2053SNP should be completed by the end of 2027.

 

Leading Brands Trust in Our Products and Services